Effect of Additive Concentration on the Dielectric Properties of Extruded HVDC Cable Insulation

Niittymäki, M.; Lähteenmäki, S.; Lahti, K.; Rytöluoto, I.; Mulakkal, M.; Diban, B.; Mazzanti, G. (2026)

 
Avaa tiedosto
Effect_of_Additive_Concentration_on_the_Dielectric_Properties_of_Extruded_HVDC_Cable_Insulation.pdf (812.6Kt)
Lataukset: 



Niittymäki, M.
Lähteenmäki, S.
Lahti, K.
Rytöluoto, I.
Mulakkal, M.
Diban, B.
Mazzanti, G.
2026

This publication is copyrighted. You may download, display and print it for Your own personal use. Commercial use is prohibited.
doi:10.1109/ICD64907.2026.11665248
Näytä kaikki kuvailutiedot
Julkaisun pysyvä osoite on
https://urn.fi/URN:NBN:fi:tuni-202609229915

Kuvaus

Peer reviewed
Tiivistelmä
In the future HVDC networks, the operational fields and temperature will also set new challenges for the insulation materials. One solution for the next-generation HVDC cable insulation material could be polypropylene (PP) based blends instead of state-of-the-art cross-linked polyethylene (XLPE). Under high DC field stress, mitigation of space charge accumulation in extruded HVDC cables is a necessity. A promising method for space charge mitigation in cable insulation material could be adding grafted additives into insulation matrix, e.g. maleic anhydride grafted PP (PP-g-MAH). This paper studies the effects of different concentrations (0.5 wt-% to 8.0 wt-%) of grafted maleic anhydride in PP cable insulation material by investigating their material and dielectric properties. No significant changes in morphological characteristics are observed with PP g MAH contents up to 8.0 wt-%. According to TSDC and PEA measurements, effective space charge mitigation is not yet achieved at 0.5 wt-%, whereas the optimal concentration could be in the range of 1.0-5.0 wt -%. Additives increase the short-term DC breakdown strength (BDS) in comparison to the reference material, but the concentration does not have significant effect on the BDS. However, the additivated PP blends have remarkably higher BDS than DC XLPE.
Kokoelmat
  • TUNICRIS-julkaisut [26236]
Kalevantie 5
PL 617
33014 Tampereen yliopisto
oa[@]tuni.fi | Tietosuoja | Saavutettavuusseloste
 

 

Selaa kokoelmaa

TekijätNimekkeetTiedekunta (2019 -)Tiedekunta (- 2018)Tutkinto-ohjelmat ja opintosuunnatAvainsanatJulkaisuajatKokoelmat

Omat tiedot

Kirjaudu sisäänRekisteröidy
Kalevantie 5
PL 617
33014 Tampereen yliopisto
oa[@]tuni.fi | Tietosuoja | Saavutettavuusseloste