Simulation of Delamination Growth at CFRP-Tungsten Aerospace Laminates Using VCCT and CZM Modelling Techniques

Jokinen, J.; Kanerva, M. (2018-06)

 
Avaa tiedosto
Jokinen_Kanerva2018_Article_SimulationOfDelaminationGrowth.pdf (2.083Mt)
Lataukset: 



Jokinen, J.
Kanerva, M.
06 / 2018

Applied Composite Materials
doi:10.1007/s10443-018-9746-5
Näytä kaikki kuvailutiedot
Julkaisun pysyvä osoite on
https://urn.fi/URN:NBN:fi:tty-201901091036

Kuvaus

Peer reviewed
Tiivistelmä
<p>Delamination analysis in advanced composites is required for the laminate design phase and also during the operation of composite aerospace structures to estimate the criticality of flaws and damage. The virtual crack closure technique (VCCT) and cohesive zone modelling (CZM) have been applied to delamination simulation as numerical tools of crack modelling. VCCT and CZM have their unique advantages and disadvantages per application. This study focuses on the application of VCCT to a brittle delamination in a hybrid tungsten–carbon-fibre reinforced composite (CFRP-W) and pursues to identify the challenges due to very high internal residual stresses and strain energy as well as unstable crack propagation. The CFRP-W composites have application areas in high-performance, light-weight radiation protection enclosures of satellite electronics and ultra-high frequency (e.g. 5G) systems. In our work, we present the effects of free-edge stress concentrations and interfacial separation prior to nodal release on a combined VCCT-CZM model and compare the results to pure VCCT and CZM models of the interfacial crack. Parameter notes are given based on the results to apply the combined method for delamination analyses with interfaces heavily loaded by internal residual strains.</p>
Kokoelmat
  • TUNICRIS-julkaisut [23896]
Kalevantie 5
PL 617
33014 Tampereen yliopisto
oa[@]tuni.fi | Tietosuoja | Saavutettavuusseloste
 

 

Selaa kokoelmaa

TekijätNimekkeetTiedekunta (2019 -)Tiedekunta (- 2018)Tutkinto-ohjelmat ja opintosuunnatAvainsanatJulkaisuajatKokoelmat

Omat tiedot

Kirjaudu sisäänRekisteröidy
Kalevantie 5
PL 617
33014 Tampereen yliopisto
oa[@]tuni.fi | Tietosuoja | Saavutettavuusseloste